Mechanical Properties Metric English Comments
Dart Drop, Total Energy 68.0 J

@Temperature 23.0 °C
50.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® BFL4000U PC (Asia Pacific)
Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo..
Dart Drop, Total Energy 68.0 J

@Temperature 23.0 °C
50.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® BFL4000U PC (Europe-Africa-Middle East)
Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo..
Dart Drop, Total Energy 68.0 J

@Temperature 23.0 °C
50.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer (Asia Pacific)
This product will be phased out per January 2015 -- Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance.
Dart Drop, Total Energy 68.0 J

@Temperature 23.0 °C
50.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer (Europe-Africa-Middle East)
This product will be phased out per January 2015 -- Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance.
Dart Drop, Total Energy 68.0 J

@Temperature 23.0 °C
50.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer
Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul..
Dart Drop, Total Energy 68.0 J

@Temperature 23.0 °C
50.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer (Asia Pacific)
Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul..
Dart Drop, Total Energy 68.0 J

@Temperature 23.0 °C
50.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® FXM2143H PC Copolymer
FXM2143H is a high flow, UV stabilized, high heat polycarbonate copolymer with an HDT/Af of 142 C.
Dart Drop, Total Energy 68.0 J

@Temperature 23.0 °C
50.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® R9453 PC (Asia Pacific)
Lexan* R9453 Polycarbonate (PC) is a non-filled, non-chlorine and non-brominate flame retardant resin for general purpose, which contains 30% post-consumer recycled PC. This resin is of UL-94 V0 rat..
Dart Drop, Total Energy 68.0 J

@Temperature 23.0 °C
50.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer
XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Dart Drop, Total Energy 68.0 J

@Temperature 23.0 °C
50.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Asia Pacific)
XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Dart Drop, Total Energy 68.0 J

@Temperature 23.0 °C
50.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Europe-Africa-Middle East)
XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Dart Drop, Total Energy 68.0 J

@Temperature 23.0 °C
50.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® XHT2143 PC Copolymer (Europe-Africa-Middle East)
XHT2143 is a high flow, UV stabilized, high heat polycarbonate copolymer with an HDT/Af of 142 C. It is available in a range of opaque and limited transparent colors.
Dart Drop, Total Energy 68.0 J

@Temperature 23.0 °C
50.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer
XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo..
Dart Drop, Total Energy 68.0 J

@Temperature 23.0 °C
50.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Europe-Africa-Middle East)
XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo..
Dart Drop, Total Energy 68.0 J

@Temperature 23.0 °C
50.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer
XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Dart Drop, Total Energy 68.0 J

@Temperature 23.0 °C
50.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Asia Pacific)
XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Dart Drop, Total Energy 68.0 J

@Temperature 23.0 °C
50.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Europe-Africa-Middle East)
XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Dart Drop, Total Energy 68.0 J

@Temperature 23.0 °C
50.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer
XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Dart Drop, Total Energy 68.0 J

@Temperature 23.0 °C
50.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer (Asia Pacific)
XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Dart Drop, Total Energy 68.0 J

@Temperature 23.0 °C
50.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer (Europe-Africa-Middle East)
XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Dart Drop, Total Energy 68.0 J

@Temperature 23.0 °C
50.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® BFL4000U PC
Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo..
Dart Drop, Total Energy 68.0 J

@Temperature 23.0 °C
50.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Asia Pacific)
XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo..
Dart Drop, Total Energy 68.0 J

@Temperature 23.0 °C
50.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics XYLEX X8419 PC+POLYESTER (Asia Pacific)
Low-medium flow, suitable for blow molding, injection molding, extrusion.
Dart Drop, Total Energy 68.0 J

@Temperature 23.0 °C
50.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics XYLEX X8419 PC+POLYESTER (Europe-Africa-Middle East)
Low-medium flow, suitable for blow molding, injection molding, extrusion.
Dart Drop, Total Energy 68.0 J
50.2 ft-lb
ASTM D3763
Lubrizol ISOPLAST™ 302EZ Engineering Thermoplastic Polyurethane Resin
NSF Standard 61 CertifiedInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.