Mechanical Properties Metric English Comments
Dart Drop, Total Energy 42.0 J
31.0 ft-lb
ASTM D3029
SABIC Innovative Plastics Cycolac® BDT6500 ABS
AUTOMOTIVE. Low gloss, color concentratable for interior applications. Natural only.
Dart Drop, Total Energy 42.0 J
31.0 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics NORYL PX9406 PPE+PS
Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 252F HDT. UL94 V-0 rated. Electrical applications.
Dart Drop, Total Energy 42.0 J
31.0 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics NORYL PX9406 PPE+PS (Asia Pacific)
Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 252F HDT. UL94 V-0 rated. Electrical applications.
Dart Drop, Total Energy 42.0 J

@Temperature 23.0 °C
31.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP NL001 PC+ABS
LNP LUBRICOMP* NL001 is a compound b ased on PC+ABS resin containing 5% PTFE. Added features include: Wear Resistant, Suitable for Thin Wall Applications.
Dart Drop, Total Energy 42.0 J

@Temperature 23.0 °C
31.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics NORYL GTX NX0031 PPE+PA
NORYL GTX* NX0031 resin is a conductive resin specially designed for electrostatic painting and powder coating applications. This material combines high impact, good flow and conductivity. The mate..
Dart Drop, Total Energy 42.0 J

@Temperature 23.0 °C
31.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP 9X11428J PPS
LNP* THERMOCOMP* 9X11428J is a compound based on Polyphenylsulfone containing Proprietary Fillers. Added features of this material include: Healthcare, Low Extractable.
Dart Drop, Total Energy 42.0 J

@Temperature 23.0 °C
31.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics NORYL EM6100 PPE+PS
PPE+PS blend. Unfilled. Good balance of flow/heat/impact. Dimensional stability. Paint adhesion. Suitable for the automotive interior market: HVAC housings, radio components. MS-DB424, WSB-M4D844-A9..
Dart Drop, Total Energy 42.0 J

@Temperature 23.0 °C
31.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS (Europe-Africa-Middle East)
Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only.
Dart Drop, Total Energy 42.0 J

@Temperature 23.0 °C
31.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS
Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only.
Dart Drop, Total Energy 42.0 J

@Temperature 23.0 °C
31.0 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS (Asia Pacific)
Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only.