Mechanical Properties Metric English Comments
Fatigue Strength 550 MPa

@# of Cycles 2.00e+6
79800 psi

@# of Cycles 2.00e+6
R=smin/smax=0.1;RT; 50% probability of failure
Outokumpu SAF 2507® Duplex Stainless Steel
Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone..