Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 550 MPa @# of Cycles 2.00e+6 |
79800 psi @# of Cycles 2.00e+6 |
R=smin/smax=0.1;RT; 50% probability of failure |
Outokumpu SAF 2507® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |