Polymer Property : Fatigue Strength = 46400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 280 - 320 MPa

@# of Cycles 1.00e+8
40600 - 46400 psi

@# of Cycles 1.00e+8
Reverse Bending (R=1)
Materion Beryllium Copper Alloy 190 Strip; 1/4HM (TM01) Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R..
Fatigue Strength 290 - 320 MPa

@# of Cycles 1.00e+8
42100 - 46400 psi

@# of Cycles 1.00e+8
Reverse Bending (R=1)
Materion Beryllium Copper Alloy 25 Strip; 1/2HT (TH02) Temper (UNS C17200)
Treatment required for max strength: 2 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 73%Superficial Hardness: 30N 58-6..
Fatigue Strength 290 - 320 MPa

@# of Cycles 1.00e+8
42100 - 46400 psi

@# of Cycles 1.00e+8
Reverse Bending (R=1)
Materion Beryllium Copper Alloy 3 Strip; HT (TH04) Temper (UNS C17510)
Treatment required for max strength: 2-3 hrs @ 480ºC or Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation after 1000 hrs @ 200°C: 75%Formability Ratio..