Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 280 - 320 MPa @# of Cycles 1.00e+8 |
40600 - 46400 psi @# of Cycles 1.00e+8 |
Reverse Bending (R=1) |
Materion Beryllium Copper Alloy 190 Strip; 1/4HM (TM01) Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R.. |
|||
Fatigue Strength | 290 - 320 MPa @# of Cycles 1.00e+8 |
42100 - 46400 psi @# of Cycles 1.00e+8 |
Reverse Bending (R=1) |
Materion Beryllium Copper Alloy 25 Strip; 1/2HT (TH02) Temper (UNS C17200) Treatment required for max strength: 2 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 73%Superficial Hardness: 30N 58-6.. |
|||
Fatigue Strength | 290 - 320 MPa @# of Cycles 1.00e+8 |
42100 - 46400 psi @# of Cycles 1.00e+8 |
Reverse Bending (R=1) |
Materion Beryllium Copper Alloy 3 Strip; HT (TH04) Temper (UNS C17510) Treatment required for max strength: 2-3 hrs @ 480ºC or Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation after 1000 hrs @ 200°C: 75%Formability Ratio.. |