Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.23 kN/m @Temperature 66.0 °C, Time 1.81e+6 sec |
7.00 pli @Temperature 151 °F, Time 504 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1099-L Nitrile High Performance Plastic Adhesives Features: It is a low viscosity grade for spray application.Fast dryingProvides strong, flexible bonds.Resists weathering, water, fuels, oil and plasticizers.Bonds vinyl extrusions and sheeting. (Ma.. |
|||
Peel Strength | 1.23 kN/m @Temperature 66.0 °C, Time 1.81e+6 sec |
7.00 pli @Temperature 151 °F, Time 504 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 4491 Nitrile Industrial Adhesive Features: Low viscosity grade for spray applicationFast dryingProvides strong, flexible bondsResists weathering, water, fuels, oil and plasticizersBonds vinyl extrusions and sheeting (May stain ligh.. |
|||
Peel Strength | 1.23 kN/m @Temperature 82.0 °C, Time 1.81e+6 sec |
7.00 pli @Temperature 180 °F, Time 504 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 5 Neoprene Contact Adhesive 3M™ Scotch-Weld™ Neoprene Contact Adhesive 5 is a sprayable contact adhesive which may be used to bond many high-pressure plastic laminates to wood, particle-board, metal and other surfacesInforma.. |
|||
Peel Strength | 1.23 kN/m @Temperature 82.0 °C, Time 1.81e+6 sec |
7.00 pli @Temperature 180 °F, Time 504 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 4475 Industrial Adhesive Features: Dries quickly to a firm bondExcellent resistance to water, plasticizer migration, many detergent and soap solutions, oils and greasesA general purpose adhesive for bonding most vinyls, cer.. |
|||
Peel Strength | 1.23 kN/m @Temperature 66.0 °C, Time 1.81e+6 sec |
7.00 pli @Temperature 151 °F, Time 504 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1099 Nitrile High Performance Plastic Adhesives Features: It is a medium viscosity grade for most brush or flow applicationsFast dryingProvides strong, flexible bonds.Resists weathering, water, fuels, oil and plasticizers.Bonds vinyl extrusions a.. |
|||
Peel Strength | 1.23 kN/m @Temperature 24.0 °C, Time 259000 sec |
7.00 pli @Temperature 75.2 °F, Time 72.0 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1870 Industrial Adhesive Features: A fast drying, highly flexible adhesive with very long tack range and good water resistanceFor bonding fabrics and most other lightweight materials with little or no tendency to stain or b.. |
|||
Peel Strength | 1.23 kN/m @Temperature 24.0 °C, Time 432000 sec |
7.00 pli @Temperature 75.2 °F, Time 120 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1870 Industrial Adhesive Features: A fast drying, highly flexible adhesive with very long tack range and good water resistanceFor bonding fabrics and most other lightweight materials with little or no tendency to stain or b.. |
|||
Peel Strength | 1.23 kN/m @Temperature 24.0 °C, Time 605000 sec |
7.00 pli @Temperature 75.2 °F, Time 168 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1870 Industrial Adhesive Features: A fast drying, highly flexible adhesive with very long tack range and good water resistanceFor bonding fabrics and most other lightweight materials with little or no tendency to stain or b.. |
|||
Peel Strength | 1.23 kN/m @Temperature 24.0 °C, Time 1.21e+6 sec |
7.00 pli @Temperature 75.2 °F, Time 336 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1870 Industrial Adhesive Features: A fast drying, highly flexible adhesive with very long tack range and good water resistanceFor bonding fabrics and most other lightweight materials with little or no tendency to stain or b.. |
|||
Peel Strength | 1.23 kN/m @Temperature 24.0 °C, Time 1.81e+6 sec |
7.00 pli @Temperature 75.2 °F, Time 504 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1870 Industrial Adhesive Features: A fast drying, highly flexible adhesive with very long tack range and good water resistanceFor bonding fabrics and most other lightweight materials with little or no tendency to stain or b.. |