Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 3.16 kN/m @Time 259000 sec |
18.0 pli @Time 72.0 hour |
Adhesion to Stainless; ASTM D3330 |
3M 4412G Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Peel Strength | 3.16 kN/m @Time 259000 sec |
18.0 pli @Time 72.0 hour |
Adhesion to Aluminum; ASTM D3330 |
3M 4412G Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Peel Strength | 3.16 kN/m @Time 259000 sec |
18.0 pli @Time 72.0 hour |
Adhesion to PC; ASTM D3330 |
3M 4412G Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Peel Strength | 3.16 kN/m @Time 259000 sec |
18.0 pli @Time 72.0 hour |
Adhesion to ABS; ASTM D3330 |
3M 4412G Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Peel Strength | 3.16 kN/m @Time 259000 sec |
18.0 pli @Time 72.0 hour |
Adhesion to PVC; ASTM D3330 |
3M 4412G Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Peel Strength | 3.16 kN/m @Temperature 24.0 °C, Time 86400 sec |
18.0 pli @Temperature 75.2 °F, Time 24.0 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1300 Neoprene High Performance Rubber Gasket Adhesives 3M™ Scotch-Weld™ Neoprene High Performance Rubber ^& Gasket Adhesives 1300 is the most versatile of our rubber and gasket adhesives. They may be used to bond metal, wood, most plastics, and neopre.. |
|||
Peel Strength | 3.16 kN/m @Temperature 24.0 °C, Time 605000 sec |
18.0 pli @Temperature 75.2 °F, Time 168 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 5 Neoprene Contact Adhesive 3M™ Scotch-Weld™ Neoprene Contact Adhesive 5 is a sprayable contact adhesive which may be used to bond many high-pressure plastic laminates to wood, particle-board, metal and other surfacesInforma.. |
|||
Peel Strength | 3.16 kN/m @Temperature 24.0 °C, Time 1.21e+6 sec |
18.0 pli @Temperature 75.2 °F, Time 336 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 5 Neoprene Contact Adhesive 3M™ Scotch-Weld™ Neoprene Contact Adhesive 5 is a sprayable contact adhesive which may be used to bond many high-pressure plastic laminates to wood, particle-board, metal and other surfacesInforma.. |
|||
Peel Strength | 3.16 kN/m @Time 259000 sec |
18.0 pli @Time 72.0 hour |
Adhesion to PC; ASTM D3330 |
3M 4411B Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Peel Strength | 3.16 kN/m @Time 259000 sec |
18.0 pli @Time 72.0 hour |
Adhesion to ABS; ASTM D3330 |
3M 4411B Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Peel Strength | 3.16 kN/m @Time 259000 sec |
18.0 pli @Time 72.0 hour |
Adhesion to Stainless; ASTM D3330 |
3M 4412N Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Peel Strength | 3.16 kN/m @Time 259000 sec |
18.0 pli @Time 72.0 hour |
Adhesion to Aluminum; ASTM D3330 |
3M 4412N Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Peel Strength | 3.16 kN/m @Time 259000 sec |
18.0 pli @Time 72.0 hour |
Adhesion to PC; ASTM D3330 |
3M 4412N Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Peel Strength | 3.16 kN/m @Time 259000 sec |
18.0 pli @Time 72.0 hour |
Adhesion to PP; ASTM D3330 |
3M 4412N Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Peel Strength | 3.16 kN/m @Temperature 24.0 °C, Time 86400 sec |
18.0 pli @Temperature 75.2 °F, Time 24.0 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1300L Neoprene High Performance Rubber Gasket Adhesives 3M™ Scotch-Weld™ Neoprene High Performance Rubber ^& Gasket Adhesives 1300 is the most versatile of our rubber and gasket adhesives. They may be used to bond metal, wood, most plastics, and neopre.. |