Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.40 - 2.63 kN/m @Temperature 24.0 °C, Time 173000 sec |
8.00 - 15.0 pli @Temperature 75.2 °F, Time 48.0 hour |
180°, Supported Vinyl/Wood |
3M Fastbond™ 4213-NF Industrial Adhesive 3M™ Fastbond™ Industrial Adhesive 4213-NF is a white, water dispersed adhesive for bonding many fabrics, supported vinyl, wood, leather and most porous materials. Exhibits outstanding clarity when.. |
|||
Peel Strength | 1.40 kN/m @Temperature 24.0 °C, Time 86400 sec |
8.00 pli @Temperature 75.2 °F, Time 24.0 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1870 Industrial Adhesive Features: A fast drying, highly flexible adhesive with very long tack range and good water resistanceFor bonding fabrics and most other lightweight materials with little or no tendency to stain or b.. |
|||
Peel Strength | 1.40 kN/m @Temperature 100 °C |
8.00 pli @Temperature 212 °F |
Bell Peel, 5 days @ 22°C/72°F, Conditioning: Dry; EN2243-2 |
Hexcel® Redux® 810 Two-Part Epoxy Paste Adhesive Redux® 810 is a multi-purpose, high shear and peel strength, two-part, toughened epoxy paste adhesive with corrosion-inhibiting properties.Features: Available in cartridges with a static mixer and .. |