Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 689 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength >= 689 MPa

@Thickness 25.4 - 38.1 mm
>= 100000 psi

@Thickness 1.00 - 1.50 in
ASTM E-8
H.C. Starck 3403 Molybdenum Alloy APT-3 TZM, Arc-Cast Plate
Arc-Cast Plate 3403Description of Product: This specification covers rolled plate of carbon-deoxidized TZM alloy (molybdenum + 0.5% titanium + 0.08% zirconium) produced from sheet bar consolidated ..
Tensile Strength >= 689 MPa

@Diameter 28.57 - 47.63 mm
>= 100000 psi

@Diameter 1.125 - 1.875 in
ASTM E-8
H.C. Starck Molybdenum Alloy PBT, Bar
Powder Metallurgy BarDescription of Product: This specification covers molybdenum alloy (Molybdenum + 0.5% titanium + 0.1% zirconium) wrought bar produced from pressed and sintered powder metallurg..
Tensile Strength >= 689 MPa

@Diameter 28.57 - 47.63 mm
>= 100000 psi

@Diameter 1.125 - 1.875 in
ASTM E-8
H.C. Starck Molybdenum Alloy TZM ABT, Arc-Cast Bar
Description of Product: This specification covers carbon-deoxidized TZM alloy (molybdenum + 0.5% titanium + 0.08% zirconium) wrought bar produced from ingots consolidated by the H.C. Starck consuma..
Tensile Strength >= 689 MPa

@Thickness 1.52 - 2.54 mm
>= 100000 psi

@Thickness 0.0600 - 0.100 in
ASTM E-8
H.C. Starck Pure Molybdenum, Sheet Premium Grade PS-100-2
Description of Product: Rolled molybdenum sheet produced from pressed and sintered powder metallurgy sheet bar.Structure: Sheet will be supplied in a stress-relieved condition unless otherwise req..
Tensile Strength >= 689 MPa

@Thickness 2.54 - 4.75 mm
>= 100000 psi

@Thickness 0.100 - 0.187 in
ASTM E-8
H.C. Starck Pure Molybdenum, Sheet Premium Grade PS-100-2
Description of Product: Rolled molybdenum sheet produced from pressed and sintered powder metallurgy sheet bar.Structure: Sheet will be supplied in a stress-relieved condition unless otherwise req..
Tensile Strength >= 689 MPa

@Thickness 1.52 - 2.54 mm
>= 100000 psi

@Thickness 0.0600 - 0.100 in
ASTM E-8
H.C. Starck 3202 Pure Molybdenum ASL, Arc-Cast, Low Carbon Sheet
Arc-Cast Sheet 3202 Low CarbonDescription of Product: This specification covers rolled sheet of carbon-deoxidized molybdenum produced from sheet bar consolidated by the H.C. Starck consumable elect..
Tensile Strength >= 689 MPa

@Thickness 2.54 - 4.75 mm
>= 100000 psi

@Thickness 0.100 - 0.187 in
ASTM E-8
H.C. Starck 3202 Pure Molybdenum ASL, Arc-Cast, Low Carbon Sheet
Arc-Cast Sheet 3202 Low CarbonDescription of Product: This specification covers rolled sheet of carbon-deoxidized molybdenum produced from sheet bar consolidated by the H.C. Starck consumable elect..
Tensile Strength 689 - 793 MPa

@Thickness <=25.4 mm
100000 - 115000 psi

@Thickness <=1.00 in
Cold Drawn Bars
Schmolz + Bickenbach UGIMA 303 UX® Stainless Steel Bar
Description: 303 UGIMA UX® is an improved machining grade produced only by Ugitech, providing the ultimate level of machinability available in an austenitic stainless steel. 303 UGIMA UX® feat..
Tensile Strength 689 - 793 MPa

@Thickness <=25.4 mm
100000 - 115000 psi

@Thickness <=1.00 in
Cold Drawn Bars
Schmolz + Bickenbach UGIMA 304/304L® Stainless Steel Bar
Description: 304/304L UGIMA® is the next generation of improved high machinability grades from Ugitech. The UGIMA® grades have redefined high machinability stainless steels, showing improvements o..
Copyright © lookpolymers.com All Rights Reserved