Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 689 MPa @Thickness 25.4 - 38.1 mm |
>= 100000 psi @Thickness 1.00 - 1.50 in |
ASTM E-8 |
H.C. Starck 3403 Molybdenum Alloy APT-3 TZM, Arc-Cast Plate Arc-Cast Plate 3403Description of Product: This specification covers rolled plate of carbon-deoxidized TZM alloy (molybdenum + 0.5% titanium + 0.08% zirconium) produced from sheet bar consolidated .. |
|||
Tensile Strength | >= 689 MPa @Diameter 28.57 - 47.63 mm |
>= 100000 psi @Diameter 1.125 - 1.875 in |
ASTM E-8 |
H.C. Starck Molybdenum Alloy PBT, Bar Powder Metallurgy BarDescription of Product: This specification covers molybdenum alloy (Molybdenum + 0.5% titanium + 0.1% zirconium) wrought bar produced from pressed and sintered powder metallurg.. |
|||
Tensile Strength | >= 689 MPa @Diameter 28.57 - 47.63 mm |
>= 100000 psi @Diameter 1.125 - 1.875 in |
ASTM E-8 |
H.C. Starck Molybdenum Alloy TZM ABT, Arc-Cast Bar Description of Product: This specification covers carbon-deoxidized TZM alloy (molybdenum + 0.5% titanium + 0.08% zirconium) wrought bar produced from ingots consolidated by the H.C. Starck consuma.. |
|||
Tensile Strength | >= 689 MPa @Thickness 1.52 - 2.54 mm |
>= 100000 psi @Thickness 0.0600 - 0.100 in |
ASTM E-8 |
H.C. Starck Pure Molybdenum, Sheet Premium Grade PS-100-2 Description of Product: Rolled molybdenum sheet produced from pressed and sintered powder metallurgy sheet bar.Structure: Sheet will be supplied in a stress-relieved condition unless otherwise req.. |
|||
Tensile Strength | >= 689 MPa @Thickness 2.54 - 4.75 mm |
>= 100000 psi @Thickness 0.100 - 0.187 in |
ASTM E-8 |
H.C. Starck Pure Molybdenum, Sheet Premium Grade PS-100-2 Description of Product: Rolled molybdenum sheet produced from pressed and sintered powder metallurgy sheet bar.Structure: Sheet will be supplied in a stress-relieved condition unless otherwise req.. |
|||
Tensile Strength | >= 689 MPa @Thickness 1.52 - 2.54 mm |
>= 100000 psi @Thickness 0.0600 - 0.100 in |
ASTM E-8 |
H.C. Starck 3202 Pure Molybdenum ASL, Arc-Cast, Low Carbon Sheet Arc-Cast Sheet 3202 Low CarbonDescription of Product: This specification covers rolled sheet of carbon-deoxidized molybdenum produced from sheet bar consolidated by the H.C. Starck consumable elect.. |
|||
Tensile Strength | >= 689 MPa @Thickness 2.54 - 4.75 mm |
>= 100000 psi @Thickness 0.100 - 0.187 in |
ASTM E-8 |
H.C. Starck 3202 Pure Molybdenum ASL, Arc-Cast, Low Carbon Sheet Arc-Cast Sheet 3202 Low CarbonDescription of Product: This specification covers rolled sheet of carbon-deoxidized molybdenum produced from sheet bar consolidated by the H.C. Starck consumable elect.. |
|||
Tensile Strength | 689 - 793 MPa @Thickness <=25.4 mm |
100000 - 115000 psi @Thickness <=1.00 in |
Cold Drawn Bars |
Schmolz + Bickenbach UGIMA 303 UX® Stainless Steel Bar Description: 303 UGIMA UX® is an improved machining grade produced only by Ugitech, providing the ultimate level of machinability available in an austenitic stainless steel. 303 UGIMA UX® feat.. |
|||
Tensile Strength | 689 - 793 MPa @Thickness <=25.4 mm |
100000 - 115000 psi @Thickness <=1.00 in |
Cold Drawn Bars |
Schmolz + Bickenbach UGIMA 304/304L® Stainless Steel Bar Description: 304/304L UGIMA® is the next generation of improved high machinability grades from Ugitech. The UGIMA® grades have redefined high machinability stainless steels, showing improvements o.. |