Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 390 MPa @Diameter 55.0 - 100 mm |
56600 psi @Diameter 2.17 - 3.94 in |
|
United Cast Bar Unibar 400-15 As Cast Continuously Cast Spheroidal Graphite Iron Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.Unibar 400-15 is not recommend.. |
|||
Tensile Strength | 390 MPa @Diameter 55.0 - 100 mm |
56600 psi @Diameter 2.17 - 3.94 in |
|
United Cast Bar Unibar 400-15 Fully Annealed Continuously Cast Spheroidal Graphite Iron Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.Unibar 400-15 is not recommend.. |
|||
Tensile Strength | >= 390 MPa @Thickness 7.90 - 12.5 mm |
>= 56600 psi @Thickness 0.311 - 0.492 in |
Temper T451; Standard EN 485-2 |
Constellium ALPLAN® 2017A High-Strength Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 2017A precision plates combine a very good dimensional stability with a high level of mechanical strength and elongation. The outstanding flatness, the low roughness and high quality of the.. |
|||
Tensile Strength | >= 390 MPa @Thickness 12.5 - 40.0 mm |
>= 56600 psi @Thickness 0.492 - 1.57 in |
Temper T451; Standard EN 485-2 |
Constellium ALPLAN® 2017A High-Strength Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 2017A precision plates combine a very good dimensional stability with a high level of mechanical strength and elongation. The outstanding flatness, the low roughness and high quality of the.. |
|||
Tensile Strength | 390 MPa @Thickness 203.2 - 254 mm |
56600 psi @Thickness 8.000 - 10.0 in |
Typical Strength |
Constellium Alumold® 350 Aluminum Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti.. |
|||
Tensile Strength | >= 390 MPa @Thickness 203.2 - 254 mm |
>= 56600 psi @Thickness 8.000 - 10.0 in |
Tempers T651 / T652 |
Constellium Alumold® 400 Aluminum The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds.. |
|||
Tensile Strength | >= 390 MPa @Thickness 60.0 - 80.0 mm |
>= 56600 psi @Thickness 2.36 - 3.15 in |
Temper T651 |
Constellium Unidal® High-Strength Rolled Precision Aluminum Plate, Milled Both Sides Unidal® precision plates offers a combination of dimensional stability and high mechanical strength. The very low internal stress reduces the risk of deformation during machining, thereby reducing .. |
|||
Tensile Strength | >= 390 MPa @Thickness 80.0 - 120 mm |
>= 56600 psi @Thickness 3.15 - 4.72 in |
Temper T651 |
Constellium Unidal® High-Strength Rolled Precision Aluminum Plate, Milled Both Sides Unidal® precision plates offers a combination of dimensional stability and high mechanical strength. The very low internal stress reduces the risk of deformation during machining, thereby reducing .. |