Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 370 MPa @Diameter 105 - 200 mm |
53700 psi @Diameter 4.13 - 7.87 in |
|
United Cast Bar Unibar 400-15 As Cast Continuously Cast Spheroidal Graphite Iron Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.Unibar 400-15 is not recommend.. |
|||
Tensile Strength | 370 MPa @Diameter 205 - 600 mm |
53700 psi @Diameter 8.07 - 23.6 in |
|
United Cast Bar Unibar 400-15 As Cast Continuously Cast Spheroidal Graphite Iron Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.Unibar 400-15 is not recommend.. |
|||
Tensile Strength | 370 MPa @Diameter 105 - 200 mm |
53700 psi @Diameter 4.13 - 7.87 in |
|
United Cast Bar Unibar 400-15 Fully Annealed Continuously Cast Spheroidal Graphite Iron Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.Unibar 400-15 is not recommend.. |
|||
Tensile Strength | 370 MPa @Diameter 205 - 600 mm |
53700 psi @Diameter 8.07 - 23.6 in |
|
United Cast Bar Unibar 400-15 Fully Annealed Continuously Cast Spheroidal Graphite Iron Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.Unibar 400-15 is not recommend.. |
|||
Tensile Strength | >= 370 MPa @Thickness 60.0 - 80.0 mm |
>= 53700 psi @Thickness 2.36 - 3.15 in |
Temper T451; Standard EN 485-2 |
Constellium ALPLAN® 2017A High-Strength Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 2017A precision plates combine a very good dimensional stability with a high level of mechanical strength and elongation. The outstanding flatness, the low roughness and high quality of the.. |