Mechanical Properties Metric English Comments
Tensile Strength 450 MPa

@Diameter 55.0 - 100 mm
65300 psi

@Diameter 2.17 - 3.94 in
United Cast Bar Unibar 500-7 Continuously Cast Spheroidal Graphite Iron
Offers higher wear resistance, strength & heat-treatment response while still possessing good machinability and excellent surface finishes. Noise and vibration damping are good in this grade.Unibar ..
Tensile Strength 450 MPa

@Thickness 15.0 - 38.1 mm
65300 psi

@Thickness 0.591 - 1.50 in
Typical Strength
Constellium Alumold® 400 Aluminum
The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds..
Tensile Strength >= 450 MPa

@Thickness 300 - 400 mm
>= 65300 psi

@Thickness 11.8 - 15.7 in
long-transverse direction
Constellium Alumold® 500 Forged Aluminum
Forged thick blocks in Alumold® 500 have been developed to provide high and consistent strength across the thickness, good dimensional stability and excellent machinability, in order to respond to ..
Tensile Strength 450 MPa

@Thickness 400 - 450 mm
65300 psi

@Thickness 15.7 - 17.7 in
long-transverse direction
Constellium Alumold® 500 Forged Aluminum
Forged thick blocks in Alumold® 500 have been developed to provide high and consistent strength across the thickness, good dimensional stability and excellent machinability, in order to respond to ..
Tensile Strength >= 450 MPa

@Thickness 325 - 400 mm
>= 65300 psi

@Thickness 12.8 - 15.7 in
Temper T652
Constellium Certal® SPC Forged Aluminum
Certal® SPC forged has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property..
Tensile Strength >= 450 MPa

@Thickness 180 - 200 mm
>= 65300 psi

@Thickness 7.09 - 7.87 in
Constellium Fortal® Aluminum Alloy
Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m..