Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 100 MPa @Strain 2.00 %, Temperature 80.0 °C |
14500 psi @Strain 2.00 %, Temperature 176 °F |
5mm/min |
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Dry) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Tensile Strength | 100 MPa @Strain 3.00 %, Temperature -20.0 °C |
14500 psi @Strain 3.00 %, Temperature -4.00 °F |
ISO 527 |
BASF Ultramid® B3S HP PA6 (Dry) Ultramid B3S HP is a easy flowing, finely crystalline, injection molding PA6 for fast processing |
|||
Tensile Strength | 100 MPa @Temperature 50.0 °C |
14500 psi @Temperature 122 °F |
ISO 527 |
BASF Ultradur B 4300 G6 30% Glass Filled PBT Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Tensile Strength | 100 MPa @Strain 1.00 %, Temperature -20.0 °C |
14500 psi @Strain 1.00 %, Temperature -4.00 °F |
ISO 527 |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |
|||
Tensile Strength | 100 MPa @Strain 2.00 %, Temperature 60.0 °C |
14500 psi @Strain 2.00 %, Temperature 140 °F |
ISO 527 |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |