Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
ISO 180-1U
Lanxess Durethan® AKV 50 H3.0 000000 Nylon 66, 50% Glass Fibers
PA 66, 50% glass fibers, injection molding, heat-ageing stabilized
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature -30.0 °C
42.8 ft-lb/in²

@Temperature -22.0 °F
ISO 180-1U
Lanxess Durethan® AKV 50 H3.0 000000 Nylon 66, 50% Glass Fibers
PA 66, 50% glass fibers, injection molding, heat-ageing stabilized
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
ISO 180-1U
Lanxess Durethan® BKV 140 DUS008 000000 Nylon 6, 40% Glass Fiber
PA 6, 40% glass fibers, injection molding, impact modifiedInformation provided by LANXESS.
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature -30.0 °C
42.8 ft-lb/in²

@Temperature -22.0 °F
ISO 180-1U
Lanxess Durethan® BKV 140 DUS008 000000 Nylon 6, 40% Glass Fiber
PA 6, 40% glass fibers, injection molding, impact modifiedInformation provided by LANXESS.
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
cond.; ISO 180-1U
Lanxess Durethan® BKV 215 H2.0 DUS008 901510 Nylon 6, Impact Modified
PA 6, 15% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
conditioned; ISO 180-1U
Lanxess Durethan® BKV 230 H2.0 DUS008 000000 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fibersInformation provided by LANXESS.
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
d.a.m.; ISO 180-1U
Lanxess Durethan® AKV 40 H3.0 000000 Nylon 66, Glass Fiber Reinforced
PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature -30.0 °C
42.8 ft-lb/in²

@Temperature -22.0 °F
d.a.m.; ISO 180-1U
Lanxess Durethan® AKV 40 H3.0 000000 Nylon 66, Glass Fiber Reinforced
PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
d.a.m.; ISO 180-1U
Lanxess Durethan® DP BKV 60 EF 000000 Nylon6, 60% Glass Fiber
PA 6, 60% glass fibers, injection molding, improved flowabilityInformation provided by LANXESS.
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
cond.; ISO 180-1U
Lanxess Durethan® DP BKV 60 EF 000000 Nylon6, 60% Glass Fiber
PA 6, 60% glass fibers, injection molding, improved flowabilityInformation provided by LANXESS.
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature -30.0 °C
42.8 ft-lb/in²

@Temperature -22.0 °F
d.a.m.; ISO 180-1U
Lanxess Durethan® DP BKV 60 EF 000000 Nylon6, 60% Glass Fiber
PA 6, 60% glass fibers, injection molding, improved flowabilityInformation provided by LANXESS.
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature -30.0 °C
42.8 ft-lb/in²

@Temperature -22.0 °F
cond.; ISO 180-1U
Lanxess Durethan® DP BKV 60 EF 000000 Nylon6, 60% Glass Fiber
PA 6, 60% glass fibers, injection molding, improved flowabilityInformation provided by LANXESS.
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp PF00A PA 6 (Europe-Africa-Middle East)
50% glass fibre reinforced Polyamide 6 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature -30.0 °C
42.8 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp PF00A PA 6 (Europe-Africa-Middle East)
50% glass fibre reinforced Polyamide 6 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
Sax Polymers SAXAMID 136F6Q32 Nylon 6, 30% Glass Fiber
SAXAMID 136F6Q32 is a high-impact-modified polyamide 6 injection-molding-grade reinforced with 30% glass fibers . Beside the high impact strength at low temperatures this grade shows very good proce..
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
Sax Polymers SAXAMID 226F7 Nylon 6.6, 35% Glass Fiber
SAXAMID 226F7 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 35% glass fibers. It has very high mechanical strength in combination with good impact resistance. It is char..
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
Sax Polymers SAXAMID 236F4Q32 Nylon 6.6, 20% Glass Fiber
SAXAMID 236 F4Q32 is a impact-modified polyamide 6.6 injection-molding-grade reinforced with 20% glass fibers and very good flow properties. It is suitable for applications requiring toughness in co..
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Sax Polymers SAXLAC 207 Acrylonitrile Butadiene Styrene
Saxalac 207 is a high heat ABS, characterized by high impact strength and high stiffness.Mechanical property data tested at 50% RH.Information provided by SAX Polymers
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature -30.0 °C
42.8 ft-lb/in²

@Temperature -22.0 °F
ISO 180
Sax Polymers SAXLAC 310A Acrylonitrile Butadiene Styrene
Saxalac 310A is a medium viscosity, impact resistant ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provid..
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
80x10x4; ISO 180/1U
Eurostar Star X 1615 33V S4 PA66, Glass Fiber Reinforced, UV stabilized, Injection Molding
Star X 1615 33V S4 is an Impact Modified, Glass Fiber Reinforced, UV stabilized Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
80x10x4; ISO 180/1U
Eurostar Staramide BG10 PA6, 50% Glass Filled, Injection Molded
BG10 is a 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature -30.0 °C
42.8 ft-lb/in²

@Temperature -22.0 °F
80x10x4; ISO 180/1U
Eurostar Staramide BG10 PA6, 50% Glass Filled, Injection Molded
BG10 is a 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
80x10x4; ISO 180/1U
Eurostar Staramide BG10H PA6, 50% Glass Filled, Injection Molded
BG10 is a Heat Stabilized, 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature -30.0 °C
42.8 ft-lb/in²

@Temperature -22.0 °F
80x10x4; ISO 180/1U
Eurostar Staramide BG10H PA6, 50% Glass Filled, Injection Molded
BG10 is a Heat Stabilized, 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
80x10x4; ISO 180/1U
Eurostar Staramide BG10HU PA6, 50% Glass Fiber Filled, UV and Heat Stabilized, Injection Molded
Staramide BG10HU is an UV and Heat Stabilized, 50% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature -30.0 °C
42.8 ft-lb/in²

@Temperature -22.0 °F
80x10x4; ISO 180/1U
Eurostar Staramide BG10HU PA6, 50% Glass Fiber Filled, UV and Heat Stabilized, Injection Molded
Staramide BG10HU is an UV and Heat Stabilized, 50% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature -30.0 °C
42.8 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1U
Eurotec® Tecomid® NA40 GR50 NL HS PA6.6, 50% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature -30.0 °C
42.8 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1U
Eurotec® Tecomid® NB40 GR30 NL MB PA6, 30% glass fiber reinforced, impact modified, heat stabilized, natural
Information provided by Eurotec®
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
Eurotec® Tecomid® NA40 GR35 NL HS PA6.6, 35% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
Izod Impact, Unnotched (ISO) 90.0 kJ/m²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
Sax Polymers SAXAMID 236F6Q32 Nylon 6.6, 30% Glass Fiber
SAXAMID 236F6Q32 is a impact-modified polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers and very good flow properties. It is suitable for applications requiring toughness in com..