Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
conditioned; ISO 180-1U |
Lanxess Durethan® AKV 35 LT H3.0 000000 Nylon 66, 35% Glass Fiber PA 66, 35% glass fiberInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
d.a.m.; ISO 180-1U |
Lanxess Durethan® BKV 130 DUS008 901510 Nylon 6, Glass Fiber Reinforced, Impact Modified PA 6, 30% glass fibers, injection molding, impact modifiedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
cond.; ISO 180-1U |
Lanxess Durethan® BKV 130 DUS008 901510 Nylon 6, Glass Fiber Reinforced, Impact Modified PA 6, 30% glass fibers, injection molding, impact modifiedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
d.a.m.; ISO 180-1U |
Lanxess Durethan® BKV 130 H2.0 DUS008 901510 Nylon 6, Glass Fiber Reinforced, Impact Modified PA 6, 30% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
cond.; ISO 180-1U |
Lanxess Durethan® BKV 130 H2.0 DUS008 901510 Nylon 6, Glass Fiber Reinforced, Impact Modified PA 6, 30% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 180-1U |
Lanxess Durethan® BKV 50 H EF DUS022 900116 Nylon 6, Glass Fiber Reinforced PA 6, 50% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 180-1U |
Lanxess Durethan® DP BKV 30 XF 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, improved flowability, improved surface finishInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 180-1U |
Lanxess Durethan® DP BKV 30 XF 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, improved flowability, improved surface finishInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 180-1U |
Lanxess Durethan® BKV 30 H2.0 EF 000000 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
ISO 180-1U |
Lanxess Durethan® BKV 325 Z H2.0 901510 Nylon 6, 25% Glass Fibers PA 6, 25% glass fibers, blow molding, impact modified, heat-ageing stabilized |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 180-1U |
Lanxess Durethan® ECO BV 35 H2 900500 Nylon 6, 35% Glass Fiber PA 6, 35% glass fibers, injection molding, heat-ageing stabilized, contains 30% pre-consumer recycled materialInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Sax Polymers SAXAMID 126F5 Nylon 6, 25% Glass Fiber SAXAMID 126F5 is a polyamide 6 injection-molding-grade reinforced with 25% glass fibers.Information provided by SAX Polymers |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Sax Polymers SAXLAC 120T Acrylonitrile Butadiene Styrene Saxalac 120T is an antistatic, easy flowing ABS injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Mechanical property data tested .. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Sax Polymers SAXLAC 120U Acrylonitrile Butadiene Styrene Saxalac 120U is an UV protected easy flowing ABS injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Mechanical property data tested.. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Sax Polymers SAXLAC 420HI Acrylonitrile Butadiene Styrene Saxalac 420HI is a flame retardant, very high flow ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provided.. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Sax Polymers SAXLAC 835U Acrylonitrile Butadiene Styrene Saxalac 835U is an antistatic, easy flowing light stabilized ABS injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Mechanical prop.. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1U |
DuPont Performance Polymers Zytel® 77G33HS1L NC010 Nylon 612 Zytel® 77G33HS1L NC010 is a 33% glass fiber reinforced, heat stabilized polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Eurotec® Tecomid® NA40 GR30 NL HS PA6.6, 30% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Eurotec® Tecomid® NA40 GR30 NL HW PA6.6, 30% glass fiber reinforced, hydrolysis stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Eurotec® Tecomid® NA40 GR30 NL RT PA6.6, 30% glass fiber reinforced, PTFE modified, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1U |
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612
(Unverified Data**) Zytel® FG77G33L NC010 is a 33% glass fiber reinforced polyamide 612 resin for injection molding. It has been developed for consideration for applications such as parts in the food industry.Informat.. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Eurotec® Tecomid® NB40 GR25 NL PA6, 25% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Sax Polymers SAXLAC 835T Acrylonitrile Butadiene Styrene Saxalac 835T is an antistatic, easy flowing ABS injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Mechanical property data tested .. |
|||
Izod Impact, Unnotched (ISO) | 70.0 kJ/m² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 180-1U |
Lanxess Durethan® BKV 35 CX H2.0 900876 Nylon 6, Glass Fiber Reinforced PA 6, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |