Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00480 GPa | 0.696 ksi | At Use Limit; ASTM C268 |
BNZ Materials Blazecrete 2600 Dense Castable Blazecrete 2600 is a general purpose castable for service to 2600°F (1427°C). It is especially effective in casting door linings, boiler walls, monolithic car tops, hearths, fire boxes, as well as.. |
|||
Modulus of Rupture | 0.00480 GPa @Temperature 104 °C |
0.696 ksi @Temperature 219 °F |
Dried; ASTM C268 |
BNZ Materials Blazecrete 3000 Dense Castable Blazecrete 3000 is a high alumina, high strength, general purpose castable for service to 3000°F (1667°C). Used for casting burner blocks, door linings, car tops, crucible furnace linings and spec.. |
|||
Modulus of Rupture | 0.00480 GPa @Temperature 540 °C |
0.696 ksi @Temperature 1000 °F |
Fired; ASTM C268 |
BNZ Materials Blazecrete 3200 Dense Castable Blazecrete 3200 is a high alumina castable for service to 3200°F (1778°C). It has good volume stability, extremely high modulus of rupture and crushing strength, and is of high purity for special .. |
|||
Modulus of Rupture | 0.00480 GPa @Temperature 815 °C |
0.696 ksi @Temperature 1500 °F |
ASTM C268 |
BNZ Materials Blazecrete 3200 Dense Castable Blazecrete 3200 is a high alumina castable for service to 3200°F (1778°C). It has good volume stability, extremely high modulus of rupture and crushing strength, and is of high purity for special .. |
|||
Modulus of Rupture | 0.00480 GPa @Temperature 1095 °C |
0.696 ksi @Temperature 2003 °F |
ASTM C268 |
BNZ Materials Blazecrete 3200 Dense Castable Blazecrete 3200 is a high alumina castable for service to 3200°F (1778°C). It has good volume stability, extremely high modulus of rupture and crushing strength, and is of high purity for special .. |