Polymer Property : Modulus of Rupture = 0.00480 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00480 GPa
0.696 ksi
At Use Limit; ASTM C268
BNZ Materials Blazecrete 2600 Dense Castable
Blazecrete 2600 is a general purpose castable for service to 2600°F (1427°C). It is especially effective in casting door linings, boiler walls, monolithic car tops, hearths, fire boxes, as well as..
Modulus of Rupture 0.00480 GPa

@Temperature 104 °C
0.696 ksi

@Temperature 219 °F
Dried; ASTM C268
BNZ Materials Blazecrete 3000 Dense Castable
Blazecrete 3000 is a high alumina, high strength, general purpose castable for service to 3000°F (1667°C). Used for casting burner blocks, door linings, car tops, crucible furnace linings and spec..
Modulus of Rupture 0.00480 GPa

@Temperature 540 °C
0.696 ksi

@Temperature 1000 °F
Fired; ASTM C268
BNZ Materials Blazecrete 3200 Dense Castable
Blazecrete 3200 is a high alumina castable for service to 3200°F (1778°C). It has good volume stability, extremely high modulus of rupture and crushing strength, and is of high purity for special ..
Modulus of Rupture 0.00480 GPa

@Temperature 815 °C
0.696 ksi

@Temperature 1500 °F
ASTM C268
BNZ Materials Blazecrete 3200 Dense Castable
Blazecrete 3200 is a high alumina castable for service to 3200°F (1778°C). It has good volume stability, extremely high modulus of rupture and crushing strength, and is of high purity for special ..
Modulus of Rupture 0.00480 GPa

@Temperature 1095 °C
0.696 ksi

@Temperature 2003 °F
ASTM C268
BNZ Materials Blazecrete 3200 Dense Castable
Blazecrete 3200 is a high alumina castable for service to 3200°F (1778°C). It has good volume stability, extremely high modulus of rupture and crushing strength, and is of high purity for special ..