Mechanical Properties Metric English Comments
Modulus of Rupture 0.00410 GPa
0.595 ksi
Dry Modulus of Rupture, 50% clay/50% flint, cast bars
Old Hickory FC-120 Tennessee Ball Clay
The FC-120 clay is a special selection for sanitaryware. It is very fast casting and is designed to use in combination with the C-33A or other finer particle size distribution clay. The FC-120 provi..
Modulus of Rupture 0.00410 GPa

@Temperature 816 °C
0.595 ksi

@Temperature 1500 °F
Zircar Ceramics AX-200 Refractory Supported Heater
ZIRCAR Refractory Supported Heater Type AX-200 consists of high temperature, helically-wound, iron-chrome-aluminum metallic alloy resistance heating elements fully embedded in a strong, highly stabl..
Modulus of Rupture 0.00410 GPa

@Temperature 1371 °C
0.595 ksi

@Temperature 2500 °F
ASTM C268
BNZ Materials Blazecrete 2600 Dense Castable
Blazecrete 2600 is a general purpose castable for service to 2600°F (1427°C). It is especially effective in casting door linings, boiler walls, monolithic car tops, hearths, fire boxes, as well as..