Material Notes:
ZIRCAR Refractory Supported Heater Type AX-200 consists of high temperature, helically-wound, iron-chrome-aluminum metallic alloy resistance heating elements fully embedded in a strong, highly stable, high temperature refractory body.AX-200 precision fabricated high temperature heaters will produce uniform, reliable heat to 1100ºC (2012ºF). They are 100% organic free and will not smoke or outgas when heated. Typical Applications:Heating source in furnaces and industrial process equipment operating to 1100ºC (2012ºF).High temperature hot plate heating element.Molten metal splash resistant heating source for launders, troughs and distribution boxes.Information provided by Zircar Ceramics.
Physical Properties Metric English Comments
Density 1.92 g/cc
0.0694 lb/in³
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00410 GPa

@Temperature 816 °C
0.595 ksi

@Temperature 1500 °F
Compressive Strength 27.6 MPa

@Temperature 816 °C
4000 psi

@Temperature 1500 °F
Thermal Properties Metric English Comments
Thermal Conductivity 0.860 W/m-K

@Temperature 538 °C
5.97 BTU-in/hr-ft²-°F

@Temperature 1000 °F
0.900 W/m-K

@Temperature 1100 °C
6.25 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Maximum Service Temperature, Air 1300 °C
2370 °F
Component Elements Properties Metric English Comments
Al2O3 47 %
47 %
CaO 8.5 %
8.5 %
Other, total <= 4.5 %
<= 4.5 %
Including TiO2
SiO2 40 %
40 %
TiO2 <= 4.5 %
<= 4.5 %