Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00340 - 0.00480 GPa | 0.493 - 0.696 ksi | |
Pyrotek SF-50 Foamed Fused Silica Insulation Board SF-50 is characterized by its uniform open cell structure which allows it to be machined to close tolerances. It can be drilled, sawed or modified with conventional tools. For quick construction o.. |
|||
Modulus of Rupture | 0.00340 GPa | 0.493 ksi | parallel to thickness |
Zircar Refractory Composites RS-A1 Refractory Sheet This product is made from Type RS-A Moldable. Type RS-A was developed as an asbestos board replacement for induction coil liners and molten metal transport, and contains no asbestos. Refractory Shee.. |
|||
Modulus of Rupture | 0.00340 GPa @Temperature 104 °C |
0.493 ksi @Temperature 219 °F |
Dried; ASTM C268 |
BNZ Materials Blazecrete 2800 Dense Castable Blazecrete 2800 is an economical, high alumina refractory for service to 2800°F (1556°C). Suitable for door linings, curbs and covers, pre-cast shapes, grey iron ladles, aluminum reverberatory fur.. |
|||
Modulus of Rupture | 0.00340 GPa @Temperature 1371 °C |
0.493 ksi @Temperature 2500 °F |
ASTM C268 |
BNZ Materials Blazecrete 2800 Dense Castable Blazecrete 2800 is an economical, high alumina refractory for service to 2800°F (1556°C). Suitable for door linings, curbs and covers, pre-cast shapes, grey iron ladles, aluminum reverberatory fur.. |
|||
Modulus of Rupture | 0.00340 GPa @Temperature 1260 °C |
0.493 ksi @Temperature 2300 °F |
ASTM C268 |
BNZ Materials Blazecrete 3000 Dense Castable Blazecrete 3000 is a high alumina, high strength, general purpose castable for service to 3000°F (1667°C). Used for casting burner blocks, door linings, car tops, crucible furnace linings and spec.. |