Mechanical Properties Metric English Comments
Modulus of Rupture 0.00340 - 0.00480 GPa
0.493 - 0.696 ksi
Pyrotek SF-50 Foamed Fused Silica Insulation Board
SF-50 is characterized by its uniform open cell structure which allows it to be machined to close tolerances. It can be drilled, sawed or modified with conventional tools. For quick construction o..
Modulus of Rupture 0.00340 GPa
0.493 ksi
parallel to thickness
Zircar Refractory Composites RS-A1 Refractory Sheet
This product is made from Type RS-A Moldable. Type RS-A was developed as an asbestos board replacement for induction coil liners and molten metal transport, and contains no asbestos. Refractory Shee..
Modulus of Rupture 0.00340 GPa

@Temperature 104 °C
0.493 ksi

@Temperature 219 °F
Dried; ASTM C268
BNZ Materials Blazecrete 2800 Dense Castable
Blazecrete 2800 is an economical, high alumina refractory for service to 2800°F (1556°C). Suitable for door linings, curbs and covers, pre-cast shapes, grey iron ladles, aluminum reverberatory fur..
Modulus of Rupture 0.00340 GPa

@Temperature 1371 °C
0.493 ksi

@Temperature 2500 °F
ASTM C268
BNZ Materials Blazecrete 2800 Dense Castable
Blazecrete 2800 is an economical, high alumina refractory for service to 2800°F (1556°C). Suitable for door linings, curbs and covers, pre-cast shapes, grey iron ladles, aluminum reverberatory fur..
Modulus of Rupture 0.00340 GPa

@Temperature 1260 °C
0.493 ksi

@Temperature 2300 °F
ASTM C268
BNZ Materials Blazecrete 3000 Dense Castable
Blazecrete 3000 is a high alumina, high strength, general purpose castable for service to 3000°F (1667°C). Used for casting burner blocks, door linings, car tops, crucible furnace linings and spec..