Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00690 GPa @Treatment Temp. 815 °C |
1.00 ksi @Treatment Temp. 1500 °F |
fired and cooled |
Pyrotek Pyrocast AR70 Low-Density Refractory Castable Pyrocast AR70 refractory castable is a high-strength, low-density refractory well suited for specific aluminum foundry applications.ApplicationsSprue Bushings for low pressure die casting Intermedia.. |
|||
Modulus of Rupture | 0.00690 GPa | 1.00 ksi | At Use Limit; ASTM C268 |
BNZ Materials Blazecrete 3000 Dense Castable Blazecrete 3000 is a high alumina, high strength, general purpose castable for service to 3000°F (1667°C). Used for casting burner blocks, door linings, car tops, crucible furnace linings and spec.. |
|||
Modulus of Rupture | 0.00690 GPa | 1.00 ksi | At Use Limit; ASTM C268 |
BNZ Materials Blazecrete 3000 G Dense Castable Blazecrete 3000 G is high alumina castable for service to 3000°F (1667°C). Used in building new and repairing old refractory linings, for gunningInformation provided by BNZ Materials Inc. |
|||
Modulus of Rupture | 0.00690 GPa @Temperature 104 °C |
1.00 ksi @Temperature 219 °F |
Dried; ASTM C268 |
BNZ Materials Blazecrete 3200 Dense Castable Blazecrete 3200 is a high alumina castable for service to 3200°F (1778°C). It has good volume stability, extremely high modulus of rupture and crushing strength, and is of high purity for special .. |
|||
Modulus of Rupture | 0.00690 - 0.0103 GPa | 1.00 - 1.49 ksi | ASTM C133 |
Ceradyne Thermo-Sil® Castable TG Fused Silica Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi.. |