Material Notes:
Pyrocast AR70 refractory castable is a high-strength, low-density refractory well suited for specific aluminum foundry applications.ApplicationsSprue Bushings for low pressure die casting Intermediate tube linings for low pressure die casting Riser inserts for gravity permanent mold casting AdvantagesLow density High strength and erosion resistance Non-wetting to molten aluminum Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00690 GPa

@Treatment Temp. 815 °C
1.00 ksi

@Treatment Temp. 1500 °F
fired and cooled
Thermal Properties Metric English Comments
Thermal Conductivity 0.300 W/m-K

@Temperature 260 °C
2.08 BTU-in/hr-ft²-°F

@Temperature 500 °F
0.330 W/m-K

@Temperature 538 °C
2.29 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Maximum Service Temperature, Air 850 °C
1560 °F
Shrinkage 0.100 %

@Temperature 760 °C
0.100 %

@Temperature 1400 °F
Component Elements Properties Metric English Comments
Al2O3 20.6 %
20.6 %
CaO 15.4 %
15.4 %
Other 7.1 %
7.1 %
SiO2 56.9 %
56.9 %
Users viewing this material also viewed the following: