Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00280 - 0.00350 GPa @Treatment Temp. 750 °C, Time 86400 sec |
0.406 - 0.508 ksi @Treatment Temp. 1380 °F, Time 24.0 hour |
|
Pyrotek Insural® 85 MASTIC Insulating Mastic for Aluminum contact Applications Insural® 85 MASTIC is an asbestos-free, durable and insulating refractory composition designed for the fabrication of launders and jointing, bedding and patching of precast refractory shapes.Advant.. |
|||
Modulus of Rupture | 0.00280 - 0.00350 GPa @Treatment Temp. 750 °C, Time 86400 sec |
0.406 - 0.508 ksi @Treatment Temp. 1380 °F, Time 24.0 hour |
|
Pyrotek Insural® GP MASTIC Insulating mastic for general-purpose refractory applications Insural® GP Mastic is an asbestos-free, durable and insulating refractory fiber composition designed for general-purpose patching and veneering applications that are not exposed to contact with mol.. |
|||
Modulus of Rupture | 0.00280 GPa @Temperature 104 °C |
0.406 ksi @Temperature 219 °F |
Dried; ASTM C268 |
BNZ Materials Blazecrete 2600 Dense Castable Blazecrete 2600 is a general purpose castable for service to 2600°F (1427°C). It is especially effective in casting door linings, boiler walls, monolithic car tops, hearths, fire boxes, as well as.. |
|||
Modulus of Rupture | 0.00280 GPa @Temperature 540 °C |
0.406 ksi @Temperature 1000 °F |
Fired; ASTM C268 |
BNZ Materials Blazecrete 3000 Dense Castable Blazecrete 3000 is a high alumina, high strength, general purpose castable for service to 3000°F (1667°C). Used for casting burner blocks, door linings, car tops, crucible furnace linings and spec.. |