Polymer Property : Modulus of Rupture = 0.00350 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00280 - 0.00350 GPa

@Treatment Temp. 750 °C,
Time 86400 sec
0.406 - 0.508 ksi

@Treatment Temp. 1380 °F,
Time 24.0 hour
Pyrotek Insural® 85 MASTIC Insulating Mastic for Aluminum contact Applications
Insural® 85 MASTIC is an asbestos-free, durable and insulating refractory composition designed for the fabrication of launders and jointing, bedding and patching of precast refractory shapes.Advant..
Modulus of Rupture 0.00280 - 0.00350 GPa

@Treatment Temp. 750 °C,
Time 86400 sec
0.406 - 0.508 ksi

@Treatment Temp. 1380 °F,
Time 24.0 hour
Pyrotek Insural® GP MASTIC Insulating mastic for general-purpose refractory applications
Insural® GP Mastic is an asbestos-free, durable and insulating refractory fiber composition designed for general-purpose patching and veneering applications that are not exposed to contact with mol..