Material Notes:
Hamilton is a fine-grained kaolin with low alkali content and high PCE. These properties make for ideal air-set refractory mortars. Halloysite content provides excellent suspension and trowel ability.Information provided by Imerys
Physical Properties Metric English Comments
Particle Size 0.50 µm
0.50 µm
69% finer than
1.0 µm
1.0 µm
83% finer than
2.0 µm
2.0 µm
89% finer than
5.0 µm
5.0 µm
95% finer than
10 µm
10 µm
98% finer than
20 µm
20 µm
99% finer than
Particle Mesh Size 325 Mesh
325 Mesh
2% retained
pH 4.0
4.0
Specific Surface Area 24 m²/g
24 m²/g
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00207 GPa
0.300 ksi
Component Elements Properties Metric English Comments
Al2O3 38.8 %
38.8 %
CaO 0.20 %
0.20 %
Carbon, C 0.030 %
0.030 %
Fe2O3 1.3 %
1.3 %
K2O 0.20 %
0.20 %
Loss on Ignition(%) 14 %

@Temperature 950 °C
14 %

@Temperature 1740 °F
MgO 0.20 %
0.20 %
Na2O 0.10 %
0.10 %
P2O5 0.10 %
0.10 %
SiO2 44 %
44 %
Sulfur, S 0.080 %
0.080 %
TiO2 1.5 %
1.5 %
Descriptive Properties Value Comments
M.B.I. (meq/100g) 4.5