Mechanical Properties Metric English Comments
Compressive Modulus 28.3 GPa

@Temperature 21.1 °C
4100 ksi

@Temperature 70.0 °F
Dry; ASTM D695
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 285 Kevlar® Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Compressive Modulus 28.3 GPa

@Temperature -53.9 °C
4100 ksi

@Temperature -65.0 °F
Dry; Vacuum/Oven Cured; SACMA 1-94
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request...
Compressive Modulus 28.3 GPa

@Temperature 177 °C
4100 ksi

@Temperature 350 °F
Wet (140°F/95% RH), 0° Direction
Renegade Materials Corporation RM-3000 Bismaleimide (BMI) 6781 S2 Glass Fabric
Developed using state-of-the-art formulating technologies, RM-3000 One Part BMI RTM Resin delivers superior hot/wet performance in airframe, missile and propulsion applications at service temperatu..