Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 28.3 GPa @Temperature 21.1 °C |
4100 ksi @Temperature 70.0 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 285 Kevlar® Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Modulus | 28.3 GPa @Temperature -53.9 °C |
4100 ksi @Temperature -65.0 °F |
Dry; Vacuum/Oven Cured; SACMA 1-94 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Compressive Modulus | 28.3 GPa @Temperature 177 °C |
4100 ksi @Temperature 350 °F |
Wet (140°F/95% RH), 0° Direction |
Renegade Materials Corporation RM-3000 Bismaleimide (BMI) 6781 S2 Glass Fabric Developed using state-of-the-art formulating technologies, RM-3000 One Part BMI RTM Resin delivers superior hot/wet performance in airframe, missile and
propulsion applications at service temperatu.. |