Polymer Property : Compressive Modulus = 19.3 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 19.3 GPa

@Temperature 93.0 °C
2800 ksi

@Temperature 199 °F
Hexcel® HexPly® F155 Epoxy Resin, 120 Glass Fabric
Hexcel designation: 120-38"-F155; Fiber: 450-1/2Information provided by HexCel
Compressive Modulus 19.3 GPa

@Temperature 24.0 °C
2800 ksi

@Temperature 75.2 °F
Warp compression
Hexcel® HexPly® F185 Epoxy Resin, K285 Kevlar Fabric
Hexcel designation: 285-38"-F185; Fiber: Kev. 49 1140Information provided by HexCel