Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hexcel® HexPly® F155 Epoxy Resin, 120 Glass Fabric

Category Polymer , Thermoset , Epoxy , Epoxy/Glass SMC
Manufacturer Hexcel
Trade Name HexPly®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® F155 Epoxy Resin, 120 Glass Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hexcel designation: 120-38"-F155; Fiber: 450-1/2Information provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 4.523 MPa

@Temperature 93.0 °C
656.0 psi

@Temperature 199 °F
Flatwise TS
5.833 MPa

@Temperature 24.0 °C
846.0 psi

@Temperature 75.2 °F
Flatwise TS
319 MPa

@Temperature 93.0 °C
46300 psi

@Temperature 199 °F
393 MPa

@Temperature 24.0 °C
57000 psi

@Temperature 75.2 °F
Tensile Modulus 17.9 GPa

@Temperature 93.0 °C
2600 ksi

@Temperature 199 °F
20.7 GPa

@Temperature 24.0 °C
3000 ksi

@Temperature 75.2 °F
Compressive Yield Strength 302 MPa

@Temperature 93.0 °C
43800 psi

@Temperature 199 °F
444 MPa

@Temperature 24.0 °C
64400 psi

@Temperature 75.2 °F
Compressive Modulus 19.3 GPa

@Temperature 93.0 °C
2800 ksi

@Temperature 199 °F
20.7 GPa

@Temperature 24.0 °C
3000 ksi

@Temperature 75.2 °F
Shear Strength 61.0 MPa
8850 psi
Compression interlaminar; RT
47.0 MPa

@Temperature 93.0 °C
6820 psi

@Temperature 199 °F
Compression interlaminar
Descriptive Properties Value Comments
Cured Thickness per Ply (cm) 0.012
Laminate
Dry Resin Content (%) 42-48
Prepreg
Fiber Volume (%) 38
Laminate
Flow (%) 8-20
Users viewing this material also viewed the following: