Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 44.1 MPa @Temperature 1100 °C |
6400 psi @Temperature 2010 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST A SUPER High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Compressive Strength | 44.1 MPa @Temperature 110 °C |
6400 psi @Temperature 230 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST SUPER Dense Castables Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range.. |
|||
Compressive Strength | >= 44.1 MPa @Temperature 1400 °C, Time 10800 sec |
>= 6400 psi @Temperature 2550 °F, Time 3.00 hour |
Cold Crushing, Specification, After firing @ 1400°C |
Sharadaa Ceramics REFPLAST 60 60% Alumina Plastic Nature of bond: Chemical-CeramicInstallation: Pneumatic rammingInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Compressive Strength | 44.1 MPa @Temperature 800 °C |
6400 psi @Temperature 1470 °F |
Cold Crushing |
Sharadaa Ceramics Sharada RFC-70 Gel Bonded Castables Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E.. |
|||
Compressive Strength | 44.1 MPa @Temperature 110 °C, Time 86400 sec |
6400 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories CTL ASP-B Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 44.1 - 53.9 MPa @Temperature 1500 °C, Time 10800 sec |
6400 - 7820 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-180 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 44.1 MPa @Temperature 110 °C, Time 86400 sec |
6400 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories HSC-15 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 44.1 MPa @Temperature 1350 °C, Time 10800 sec |
6400 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HSC-15 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 44.1 MPa @Treatment Temp. 540 °C |
6400 psi @Treatment Temp. 1000 °F |
Cold Crush Strength; Dried 104°C |
BNZ Materials Blazecrete 2500 HS Dense Castable Blazecrete 2500 HSis a high-duty castable designed to withstand loads and resist normal abrasion and erosion at moderate temperatures to 2500°F (1371°C). Use with Blaz 2100 for a dual component li.. |