Chosun Refractories HSC-15 Dense and High-Strength Castable, Credens

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories HSC-15 Dense and High-Strength Castable, Credens.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00981 GPa

@Temperature 110 °C,
Time 86400 sec
1.42 ksi

@Temperature 230 °F,
Time 24.0 hour
0.00981 GPa

@Temperature 1350 °C,
Time 10800 sec
1.42 ksi

@Temperature 2460 °F,
Time 3.00 hour
Compressive Strength 44.1 MPa

@Temperature 110 °C,
Time 86400 sec
6400 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
44.1 MPa

@Temperature 1350 °C,
Time 10800 sec
6400 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1500 °C
2730 °F
limited
Shrinkage -0.0500 %

@Temperature 110 °C,
Time 86400 sec
-0.0500 %

@Temperature 230 °F,
Time 24.0 hour
-0.0500 %

@Temperature 1350 °C,
Time 10800 sec
-0.0500 %

@Temperature 2460 °F,
Time 3.00 hour
Component Elements Properties Metric English Comments
Al2O3 50 %
50 %
CaO 2.0 %
2.0 %
SiO2 45 %
45 %
Processing Properties Metric English Comments
Cure Time 120 - 600 min
2.00 - 10.0 hour
Setting Time
Descriptive Properties Value Comments
Installation Method Vibrating, Casting
Material Required for Estimating(kg/?) 2,400
Water Required for Casting(%) 8