Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 31.0 MPa @Strain 1 % |
4500 psi @Strain 1 % |
ISO 604 |
Quadrant EPP Duratron® PEI U1000 PEI, unfilled, extruded (ISO Data) Duratron U1000 PEI is an amber translucent (non-optical quality) amorphous thermoplastic material, offering high strength and heat resistance. It performs continuously to 170 °C, making it ideal fo.. |
|||
Compressive Strength | 31.0 MPa @Strain 1 % |
4500 psi @Strain 1 % |
ISO 604 |
Quadrant EPP Ertalon® 4.6 PA 4.6, extruded (ISO Data) Compared with conventional nylons, Ertalon 4.6 features a better retention of stiffness and creep resistance over a wide range of temperatures as well as superior heat ageing resistance. Therefore, .. |
|||
Compressive Strength | 31.0 MPa @Strain 1 % |
4500 psi @Strain 1 % |
ISO 604 |
Quadrant EPP Ertalon® 6 SA PA 6, extruded (ISO Data) This material offers an optimal combination of mechanical strength, stiffness, toughness, mechanical damping properties and wear resistance. These properties, together with good electrical insulatin.. |
|||
Compressive Strength | 31.0 MPa @Strain 1 % |
4500 psi @Strain 1 % |
ISO 604 |
Quadrant EPP Ertalon® LFX PA 6 + oil, cast (ISO Data) This internally lubricated cast nylon 6 is self-lubricating in the real meaning of the word. Ertalon LFX, especially developed for unlubricated, highly loaded and slow moving parts applications, yie.. |
|||
Compressive Strength | 31.0 MPa @Strain 1 % |
4500 psi @Strain 1 % |
ISO 604 |
Quadrant EPP Ertalyte® TX PET + solid lubricant, extruded (ISO Data) Ertalyte TX is a polyethylene terephthalate compound incorporating a uniformly dispersed solid lubricant. Its specific formulation makes it a premium internally lubricated bearing-grade. Ertalyte TX.. |
|||
Compressive Strength | 31.0 MPa @Strain 1 % |
4500 psi @Strain 1 % |
ISO 604 |
Quadrant EPP Ketron® TX PEEK + solid lubricant, extruded (ISO Data) This member of the Ketron PEEK family has been developed especially for the food industry. Like Ketron PEEK-1000, this new internally lubricated material has a food contact compliant composition, bu.. |
|||
Compressive Strength | 31.0 MPa @Strain 1 % |
4500 psi @Strain 1 % |
ISO 604 |
Quadrant EPP Nylatron® LFG PA 6 + oil, cast (ISO Data) Nylatron LFG (Lubricated Food Grade) is self-lubricating in the real meaning of the word, and has a FDA food contact compliant composition. The Nylatron LFG has been specially developed for non-lubr.. |
|||
Compressive Strength | 31.0 MPa @Strain 1 % |
4500 psi @Strain 1 % |
ISO 604 |
Quadrant EPP Nylatron® NSM PA 6 + internal lubricant, cast (ISO Data) Nylatron NSM is a proprietary cast nylon 6 formulation containing solid lubricant additives which grant this materials self-lubricity, excellent frictional behaviour, superior wear resistance and ou.. |
|||
Compressive Strength | 31.0 MPa @Temperature 110 °C |
4500 psi @Temperature 230 °F |
|
Pyrotek Pyrocast PT-190 Refractory Cast Parts Pyrocast PT-190 is an extremely dense alumina based refractory. It is best suited for applications where high velocity metal erosion potential is a problem, due to its strength and abrasion resista.. |
|||
Compressive Strength | 31.0 MPa @Temperature 149 °C |
4500 psi @Temperature 300 °F |
ASTM D 695 |
Saint-Gobain Meldin® 1357 Thermoplastic Bearing Material Meldin 1357 offers the lowest wear rate and coefficient of friction, which makes it the best candidate for tribological applications. In addition, its self-lubricating properties allow it to operat.. |