Mechanical Properties Metric English Comments
Compressive Strength 30.0 MPa

@Strain 4.00 %,
Temperature 23.0 °C
4350 psi

@Strain 4.00 %,
Temperature 73.4 °F
X direction, Condition A; ASTM D695
Rogers Corporation RT/duroid® 5870 Glass Microfiber Reinforced PTFE High Frequency Laminate
RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to..
Compressive Strength 30.0 MPa

@Temperature 200 °C
4350 psi

@Temperature 392 °F
ISO 604
Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia..
Compressive Strength 30.0 - 40.0 MPa

@Temperature 100 °C
4350 - 5800 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 110 C Dense Refractory Castable
Description: Curon 110 C is a coarse castable. Application: covers for anode baking furnaces.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Compressive Strength 30.0 - 40.0 MPa

@Temperature 100 °C
4350 - 5800 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 120 C Dense Refractory Castable
Description: A general purpose castable for use up to 1200°C under normal operating conditions. Curon 120 C has good thermal shock resistance.Remarks: These values apply to cast products.Informat..
Compressive Strength 30.0 - 40.0 MPa

@Temperature 100 °C
4350 - 5800 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 130 Dense Refractory Castable
Description: Curon 130 is a castable with a good workability and a high strength. Therefore this castable can be characterized as a reliable refractory construction material.Remarks: These values ap..
Compressive Strength 30.0 - 40.0 MPa

@Temperature 1600 °C
4350 - 5800 psi

@Temperature 2910 °F
Cold Crushing Strength
Gouda Vuurvast CURON 160 C Dense Refractory Castable
Description: Because of the selection of raw materials this castable has a high volume stability and keeps its strength up to high temperatures. In addition Curon 160 C has an excellent thermal shoc..
Compressive Strength 30.0 - 40.0 MPa

@Temperature 1000 °C
4350 - 5800 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast CURON 130 HRC Dense Refractory Castable
Description: A coarse, low iron castable for use up to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRC has a good thermal shock resistance becaus..
Compressive Strength 30.0 - 40.0 MPa

@Temperature 1000 °C
4350 - 5800 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast CURON 130 HRCC RAPID Dense Refractory Castable
Description: An extra coarse, low iron castable for use to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRCC RAPID has good thermal shock resistan..
Compressive Strength 30.0 - 40.0 MPa

@Temperature 100 °C
4350 - 5800 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 150 GM Dense Refractory Castable
Description: Curon 150 GM is a gunmix based on sintered bauxite with an excellent thermal shock resistance and is therefore very well suited for burner blocks.Remarks: These values apply to cast pro..
Compressive Strength 30.0 - 40.0 MPa

@Temperature 1400 °C
4350 - 5800 psi

@Temperature 2550 °F
Cold Crushing Strength
Gouda Vuurvast CURON 150 HR GM Dense Refractory Castable
Description: Curon 150 HR GM is a gunning castable, because of its low iron content also very well suitable under reducing circumstances. In addition, this castable has a good thermal shock resistan..
Compressive Strength 30.0 MPa

@Temperature 200 °C
4350 psi

@Temperature 392 °F
Result based on HT G22; ISO 604