Material Notes:
Description: Curon 150 HR GM is a gunning castable, because of its low iron content also very well suitable under reducing circumstances. In addition, this castable has a good thermal shock resistance because of its low thermal expansion.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.10 - 2.20 g/cc
0.0759 - 0.0795 lb/in³
After drying at 110°C
Particle Size <= 4000 µm
<= 4000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 30.0 - 40.0 MPa

@Temperature 1400 °C
4350 - 5800 psi

@Temperature 2550 °F
Cold Crushing Strength
35.0 - 45.0 MPa

@Temperature 100 °C
5080 - 6530 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.520 - 0.620 W/m-K

@Temperature 100 °C
3.61 - 4.30 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.570 - 0.670 W/m-K

@Temperature 600 °C
3.96 - 4.65 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.650 - 0.750 W/m-K

@Temperature 1400 °C
4.51 - 5.20 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Maximum Service Temperature, Air 1500 °C
2730 °F
Shrinkage -0.500 - 0.500 %

@Temperature 1400 °C
-0.500 - 0.500 %

@Temperature 2550 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 57 %
57 %
Fe2O3 0.60 %
0.60 %
SiO2 38 %
38 %
Descriptive Properties Value Comments
ASTM Classification D
Material Consumption per 1 m3 2050 kg