Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 26.0 MPa @Strain 1 % |
3770 psi @Strain 1 % |
ISO 604 |
Quadrant EPP Ertacetal® H-TF POM-H, PTFE-filled, extruded (ISO Data) Ertacetal H-TF is a DELRIN® AF Blend, a combination of TEFLON® fibres evenly dispersed in a DELRIN acetal resin. Much of the strength that is inherent in Ertacetal H is retained. Some properties c.. |
|||
Compressive Strength | 26.0 MPa @Strain 1 % |
3770 psi @Strain 1 % |
ISO 604 |
Quadrant EPP Nylatron® 703XL PA 6 + internal lubricant, cast (ISO Data) This high performance cast nylon 6 bearing grade provides an even better wear resistance than Nylatron NSM, combined with good pressure-velocity capabilities and a near zero level of “stick-slip”... |
|||
Compressive Strength | 26.0 MPa @Strain 2 % |
3770 psi @Strain 2 % |
ISO 604 |
Quadrant EPP Symalit® 1000 ECTFE, unfilled, lining industries (ISO Data) Symalit 1000 ECTFE is made from a fluoropolymer resin that is a copolymer of ethylene and chlorotrifluoroethylene. It exhibits good mechanical properties combined with an excellent chemical resistan.. |
|||
Compressive Strength | 26.0 MPa @Temperature 800 °C, Time 10800 sec |
3770 psi @Temperature 1470 °F, Time 3.00 hour |
Cold Crushing, Typical Value, After firing @ 800°C |
Sharadaa Ceramics REFPLAST 60 60% Alumina Plastic Nature of bond: Chemical-CeramicInstallation: Pneumatic rammingInformation provided by Sharadaa Ceramics Pvt. Ltd. |