Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 110 MPa @Temperature 1095 °C |
16000 psi @Temperature 2003 °F |
|
Pyrotek Pyrocast PT-190 Refractory Cast Parts Pyrocast PT-190 is an extremely dense alumina based refractory. It is best suited for applications where high velocity metal erosion potential is a problem, due to its strength and abrasion resista.. |
|||
Compressive Strength | 110 MPa @Temperature 120 °C |
16000 psi @Temperature 248 °F |
ISO 604 |
Victrex® PEEK 450FC30 General Purpose Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and ext.. |
|||
Compressive Strength | 110 MPa @Temperature 150 °C |
16000 psi @Temperature 302 °F |
ASTM D-695 |
Glastic GLASTHERM S Insulation Sheet Glastherm Grade S is a general purpose insulation sheet with an economical combination of thermal and physical properties. Not recommended for processes where the continuous operating temperature e.. |
|||
Compressive Strength | 110 - 130 MPa @Temperature 1000 °C |
16000 - 18900 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast FLUCON 160 K Dense Self Flowing Refractory Castable Description: Flucon 160 K is a self-flowing low cement castable based on silicon carbide. This castable is characterized by high strength high abrasion resistance and excellent thermal shock resista.. |
|||
Compressive Strength | 110 - 130 MPa @Temperature 1300 °C |
16000 - 18900 psi @Temperature 2370 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 150 G Dense Vibrating Refractory Castable Description: Vibron 150 G is a low cement castable based on sintered South-American bauxite. Especially suited for direct contact with liquid aluminum metal.Remarks: Indicated values apply to vibrat.. |
|||
Compressive Strength | 110 MPa @Temperature 23.0 °C |
16000 psi @Temperature 73.4 °F |
|
Elisto THERMOSTAR® HD 550 C Frame Press Insulation Material Pattern material. Insulation materials for mechanical engineering.Information provided by elisto |
|||
Compressive Strength | 110 MPa @Temperature 120 °C |
16000 psi @Temperature 248 °F |
ISO 604 |
Victrex® PEEK 150FC30 Easy Flow Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy .. |