Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gouda Vuurvast FLUCON 160 K Dense Self Flowing Refractory Castable

Category Ceramic , Carbide
Manufacturer Gouda Vuurvast
Trade Name FLUCON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast FLUCON 160 K Dense Self Flowing Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Flucon 160 K is a self-flowing low cement castable based on silicon carbide. This castable is characterized by high strength high abrasion resistance and excellent thermal shock resistance.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.60 - 2.70 g/cc
0.0939 - 0.0975 lb/in³
After drying at 110°C
Particle Size <= 3000 µm
<= 3000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 65.0 - 75.0 MPa

@Temperature 100 °C
9430 - 10900 psi

@Temperature 212 °F
Cold Crushing Strength
110 - 130 MPa

@Temperature 1000 °C
16000 - 18900 psi

@Temperature 1830 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 5.30 - 7.30 W/m-K

@Temperature 1000 °C
36.8 - 50.7 BTU-in/hr-ft²-°F

@Temperature 1830 °F
6.50 - 8.50 W/m-K

@Temperature 600 °C
45.1 - 59.0 BTU-in/hr-ft²-°F

@Temperature 1110 °F
8.00 - 10.0 W/m-K

@Temperature 100 °C
55.5 - 69.4 BTU-in/hr-ft²-°F

@Temperature 212 °F
Maximum Service Temperature, Air 1600 °C
2910 °F
Shrinkage -0.200 - 0.200 %

@Temperature 1000 °C
-0.200 - 0.200 %

@Temperature 1830 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Fe2O3 0.20 %
0.20 %
SiC 70 %
70 %
SiO2 7.0 %
7.0 %
Descriptive Properties Value Comments
Material Consumption per 1 m3 2600 kg
Mixing Water 5-5.5 liters
per 100 kgs dry material
Users viewing this material also viewed the following: