Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 4.90 - 14.7 MPa @Temperature 110 °C, Time 86400 sec |
711 - 2130 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories INCT-140 Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 14.7 MPa @Temperature 500 °C, Time 10800 sec |
711 - 2130 psi @Temperature 932 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories INCT-140 Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 14.7 MPa @Temperature 1000 °C, Time 10800 sec |
711 - 2130 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories INCT-140 Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 14.7 MPa @Temperature 110 °C, Time 86400 sec |
711 - 2130 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories INCT-160 Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 14.7 MPa @Temperature 1000 °C, Time 10800 sec |
711 - 2130 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories INCT-160 Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 14.7 MPa @Temperature 1350 °C, Time 10800 sec |
711 - 2130 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories INCT-170 Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 4.90 - 14.7 MPa @Temperature 1000 °C, Time 10800 sec |
711 - 2130 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories MIX-1(1:4) Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 6.86 - 14.7 MPa @Temperature 110 °C, Time 86400 sec |
996 - 2130 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories PTC-130S Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |