Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 3.85e-7 - 0.000981 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000558 - 0.142 ksi

@Temperature 230 °F,
Time 24.0 hour
0.03924 - 0.07848 GPa

@Temperature 1300 °C,
Time 10800 sec
5.691 - 11.38 ksi

@Temperature 2370 °F,
Time 3.00 hour
Compressive Strength 6.86 - 14.7 MPa

@Temperature 110 °C,
Time 86400 sec
996 - 2130 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
9.81 - 17.7 MPa

@Temperature 1300 °C,
Time 10800 sec
1420 - 2560 psi

@Temperature 2370 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.5819 W/m-K

@Temperature 500 °C
10.961 BTU-in/hr-ft²-°F

@Temperature 932 °F
Maximum Service Temperature, Air 1300 °C
2370 °F
limited
Shrinkage -0.500 %

@Temperature 110 °C,
Time 86400 sec
-0.500 %

@Temperature 230 °F,
Time 24.0 hour
1.5 %

@Temperature 1500 °C,
Time 10800 sec
1.5 %

@Temperature 2730 °F,
Time 3.00 hour
Component Elements Properties Metric English Comments
Cr2O3 25 - 30 %
25 - 30 %
Descriptive Properties Value Comments
Main Applications Dust Incinerator
Material Required for Estimating (kg/?) 2,900