Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 13.0 - 19.0 MPa @Temperature 1000 °C |
1890 - 2760 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 125 GM Refractory Insulating Castable Description: This insulating castable is characterized by a good mechanical strength and thermal shock resistance.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast... |
|||
Compressive Strength | 13.0 - 19.0 MPa @Temperature 1000 °C |
1890 - 2760 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 125 Refractory Insulating Castable Description: This insulating castable is characterized by a good mechanical strength and thermal shock resistance.Remarks: These values apply to cast products. Also available in gunning variety, mar.. |
|||
Compressive Strength | 13.0 - 19.0 MPa @Temperature 1370 °C |
1890 - 2760 psi @Temperature 2500 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 140 Refractory Insulating Castable Description: This castable is characterized by its low Fe2O3 content and its relatively high strength. Golite 140 is therefore widely applied at places with reducing or corrosive atmosphere.Remarks:.. |
|||
Compressive Strength | 13.0 - 19.0 MPa @Temperature 1260 °C |
1890 - 2760 psi @Temperature 2300 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 145 Refractory Insulating Castable Description: Golite 145 can be used in direct contact with the furnace conditions and combines a high strength with a good thermal insulation.Remarks: These values apply to cast products. Also avail.. |
|||
Compressive Strength | 13.0 - 17.0 MPa @Temperature 1500 °C |
1890 - 2470 psi @Temperature 2730 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 180 Refractory Insulating Castable Description: Hollow alumina spheres are used as an aggregate for this castable. With very low percentages of Fe2O3 and SiO2, it is well resistant against reducing and corrosive kiln atmospheres.Rema.. |
|||
Compressive Strength | 13.0 - 17.0 MPa @Temperature 100 °C |
1890 - 2470 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast GOLITE 135 GM Refractory Insulating Castable Description: This gunning material can be used in direct contact with open fire and has a high strength.Remarks: These values were obtained from cast samples. These values apply to cast products.Inf.. |