Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 13.0 - 19.0 MPa

@Temperature 1000 °C
1890 - 2760 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast GOLITE 125 GM Refractory Insulating Castable
Description: This insulating castable is characterized by a good mechanical strength and thermal shock resistance.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast...
Compressive Strength 13.0 - 19.0 MPa

@Temperature 1000 °C
1890 - 2760 psi

@Temperature 1830 °F
Cold Crushing Strength
Gouda Vuurvast GOLITE 125 Refractory Insulating Castable
Description: This insulating castable is characterized by a good mechanical strength and thermal shock resistance.Remarks: These values apply to cast products. Also available in gunning variety, mar..
Compressive Strength 13.0 - 19.0 MPa

@Temperature 1370 °C
1890 - 2760 psi

@Temperature 2500 °F
Cold Crushing Strength
Gouda Vuurvast GOLITE 140 Refractory Insulating Castable
Description: This castable is characterized by its low Fe2O3 content and its relatively high strength. Golite 140 is therefore widely applied at places with reducing or corrosive atmosphere.Remarks:..
Compressive Strength 13.0 - 19.0 MPa

@Temperature 1260 °C
1890 - 2760 psi

@Temperature 2300 °F
Cold Crushing Strength
Gouda Vuurvast GOLITE 145 Refractory Insulating Castable
Description: Golite 145 can be used in direct contact with the furnace conditions and combines a high strength with a good thermal insulation.Remarks: These values apply to cast products. Also avail..