Compressive Strength 1.47 - 2.45 MPa

@Temperature 1000 °C,
Time 10800 sec
213 - 356 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories MIX-2 Light-Weight Gunning Castable