Chosun Refractories INCT-80S Light-Weight Castable

Category Ceramic
Manufacturer Chosun Refractories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories INCT-80S Light-Weight Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 6.74e-8 - 0.000196 GPa

@Temperature 110 °C,
Time 86400 sec
0.00000977 - 0.0285 ksi

@Temperature 230 °F,
Time 24.0 hour
0.0001962 - 0.0006867 GPa

@Temperature 500 °C,
Time 10800 sec
0.02846 - 0.09960 ksi

@Temperature 932 °F,
Time 3.00 hour
Compressive Strength 0.392 - 1.37 MPa

@Temperature 110 °C,
Time 86400 sec
56.9 - 199 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
0.392 - 1.37 MPa

@Temperature 500 °C,
Time 10800 sec
56.9 - 199 psi

@Temperature 932 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.1396 W/m-K

@Temperature 260 °C
0.9671 BTU-in/hr-ft²-°F

@Temperature 500 °F
0.2210 W/m-K

@Temperature 540 °C
1.531 BTU-in/hr-ft²-°F

@Temperature 1000 °F
0.233 W/m-K

@Temperature 1000 °C
1.61 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Maximum Service Temperature, Air 800 °C
1470 °F
limited
Shrinkage -0.500 %

@Temperature 1350 °C,
Time 10800 sec
-0.500 %

@Temperature 2460 °F,
Time 3.00 hour
-0.0600 %

@Temperature 110 °C,
Time 86400 sec
-0.0600 %

@Temperature 230 °F,
Time 24.0 hour
Component Elements Properties Metric English Comments
Al2O3 28 %
28 %
SiO2 38 %
38 %
Descriptive Properties Value Comments
Installation Method Casting, Troweling
Main Applications Low temperature Various furnaces
Material Required for Estimating (kg/?) 450
Water Required for Casting(%) 140-150