Polymer Property : Tensile Modulus = 8800 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 60.7 GPa

@Temperature 21.1 °C
8800 ksi

@Temperature 70.0 °F
0° Direction, Dry; ASTM D638
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 3K PW Carbon Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Tensile Modulus 60.7 GPa

@Temperature 24.0 °C
8800 ksi

@Temperature 75.2 °F
Hexcel® HexPly® F263 Epoxy Resin, W3T282 Carbon Fabric
Hexcel designation: W3T282-42"-F263; Fiber: T300 CelionInformation provided by HexCel
Tensile Modulus 60.7 GPa

@Temperature 177 °C
8800 ksi

@Temperature 351 °F
T300, Plain Weave; Fill Tension; Wet
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Fabric Form
Fiber: T300-3KInformation provided by HexCel