Mechanical Properties Metric English Comments
Tensile Modulus 4.10 GPa

@Temperature 90.0 °C
595 ksi

@Temperature 194 °F
LATI Lastilac SP G/17 ABS, Glass Fiber Reinforced
Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Glass fibers. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInforma..
Tensile Modulus 4.10 GPa

@Temperature 150 °C
595 ksi

@Temperature 302 °F
LATI Lapex A G/10 PES, 10% Glass Fiber Reinforced
Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ..
Tensile Modulus 4.10 GPa

@Temperature 120 °C
595 ksi

@Temperature 248 °F
LATI Later 4 G/30 PBT, 30% Glass Fiber Reinforced
Polybutylene Terephthalate (PBT) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast..
Tensile Modulus 4.10 GPa

@Temperature 90.0 °C
595 ksi

@Temperature 194 °F
LATI Later 4 G/30-V0HF1 PBT, 30% Glass Fiber Reinforced, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe..
Tensile Modulus 4.10 GPa

@Temperature 90.0 °C
595 ksi

@Temperature 194 °F
LATI Kelon® A H CEG/40 PA 66, Glass/Mineral Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati..