Polymer Property : Tensile Modulus = 405 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.79 GPa

@Thickness 1.50 mm,
Temperature 120 °C
405 ksi

@Thickness 0.0591 in,
Temperature 248 °F
BASF Ultraform N 2320 003 UNC Q600 POM
Ultraform N 2320 003 UNC Q600 is a rapidly solidifying grade of POM for injection molding. Contains a mold release agent.