Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.79 GPa @Thickness 1.50 mm, Temperature 120 °C |
405 ksi @Thickness 0.0591 in, Temperature 248 °F |
|
BASF Ultraform N 2320 003 UNC Q600 POM Ultraform N 2320 003 UNC Q600 is a rapidly solidifying grade of POM for injection molding. Contains a mold release agent. |